Yield, %1 | ||||
---|---|---|---|---|
Substrates | Pretreatment conditions | Glucan | Xylan | Lignin |
Untreated corn stover | NA2 | 39.1 ± 0.4 | 23.7 ± 0.3 | 19.3 ± 0.5 |
Dilute acid-pretreated | 140°C, 1% sulfuric acid, 40 minutes | 57.6 ± 0.2 | 5.7 ± 0.7 | 22.1 ± 0.4 |
AFEX3-pretreated | 90°C, 220 psi, 1:1 NH3 to Biomass, 5 minutes | 39.6 ± 0.5 | 24.5 ± 0.4 | 18.2 ± 0.9 |