Table 2 Coded and actual levels of variables chosen for the statistical design of experiment.

From: Cellulose accessibility limits the effectiveness of minimum cellulase loading on the efficient hydrolysis of pretreated lignocellulosic substrates

Factors

Level

Pretreatment

  

SO2steama

Ethanol organosolv

  

CS,bDF,cLPd

CFe

CF

LP, Pf

Solids loading, %

-1

2

2

2

2

 

0

6

6

6

6

 

1

10

10

10

10

Hydrolysis time, hours

-1

24

24

24

24

 

0

48

48

48

48

 

1

72

72

72

72

Cellulase,g mg protein/g glucan

-1

25

5

13

20

 

0

50

15

26

45

 

1

75

25

39

70

β-glucosidase,h mg protein/g glucan

-1

0

0

0

0

 

0

15

15

10

10

 

1

30

30

20

20

  1. aSO = sulfur dioxide.
  2. bCS = corn stover.
  3. cDF = douglas fir.
  4. dLP = lodgepole pine.
  5. eCF = corn fiber.
  6. fP = poplar.
  7. gCelluclast 1.5L.
  8. hNovozym 188.