Table 2 Initial average fiber dimensions for pretreated woody substrates

From: The enzymatic hydrolysis of pretreated pulp fibers predominantly involves “peeling/erosion” modes of action

Sample

Fiber length (μm)

Fiber width (μm)

SPP200 R20

426.0(23.1)

25.20(0.42)

SPP200 R40

316.5(19.1)

24.65(0.63)

SPP180 R20

764.0(45.3)

26.95(0.36)

SPDF R100

372.5(9.2)

29.55(0.73)

SPDF F100

148.0(0.4)

25.85(0.49)

OPLP R20

1853.5(7.8)

32.15(0.22)

  1. Numbers in parentheses indicate the standard deviation.