Skip to main content

Table 1 The crystallinity indexes of the raw fiber, hydrothermal pretreated fibers, and the cellulose-rich fractions obtained after the synergistic treatment

From: Improving the enzymatic hydrolysis of thermo-mechanical fiber from Eucalyptus urophylla by a combination of hydrothermal pretreatment and alkali fractionation

 

XRD-CrI (%)

NMR-CrI (%)

 

XRD-CrI (%)

NMR-CrI (%)

RM

57.02

43.71

AM

59.79

46.45

R100-60

57.52

45.26

AR100-60

63.06

46.47

R120-60

58.31

46.39

AR120-60

65.24

46.66

R140-60

60.83

46.79

AR140-60

66.30

47.22

R160-60

62.98

49.69

AR160-60

66.75

50.74

R180-15

67.04

50.59

AR180-15

67.90

52.73

R180-30

68.05

51.48

AR180-30

68.23

52.83

R180-45

68.15

51.71

AR180-45

69.23

52.97

R180-60

69.78

53.45

AR180-60

69.26

53.53

R200-30

70.88

54.41

AR200-30

69.91

54.37

R220-30

71.75

55.79

AR220-30

72.94

54.82

R240-30

68.74

53.86

AR240-30

71.53

50.75