Fig. 2From: A biorefinery scheme to fractionate bamboo into high-grade dissolving pulp and ethanol Comparison of hemicellulose content of pulps from different treatments. a Xylanase treatment at temperature 60 °C, pH 6, and 10% pulp consistency; b CCE at temperature 30 °C and 10% pulp consistency for 45 minBack to article page