Fig. 3From: A biorefinery scheme to fractionate bamboo into high-grade dissolving pulp and ethanolHemicellulose content of pulps from the sequential treatment process of xylanase and CCE. Xylanase treatment: temperature 60 °C, pH 6, pulp consistency 10%; CCE process: temperature 30 °C, time 45 min, pulp consistency 10%. 4–12% means the used NaOH concentration during CCE processBack to article page