Skip to main content

Table 2 Overview of hydrolysis yields for various degradation reactions

From: Enzymatic degradation of sulfite-pulped softwoods and the role of LPMOs

Raw material

Enzyme

Conditions

AscA

Sulfite (12.5 mM)

Glucan solubilization after 48 h (% of theoretical)

Avicel PH-101

Cellic® CTec3

Aerobic

+

69.0 ± 1.9

Aerobic

+

+

31.6 ± 0.4

Anaerobic

+

50.0 ± 1.4

Anaerobic

+

+

44.1 ± 1.2

Celluclast®:Novozym 188

Aerobic

+

55.6 ± 0.9

Aerobic

+

+

39.5 ± 0.5

Anaerobic

+

57.1 ± 0.7

Anaerobic

+

+

38.6 ± 4.3

Norway spruce

Cellic® CTec3

Aerobic

+

73.7 ± 0.7

Aerobic

+

+

34.1 ± 0.4

Anaerobic

+

50.6 ± 3.8

Anaerobic

+

+

55.6 ± 2.3

Celluclast®:Novozym 188

Aerobic

+

64.9 ± 2.1

Aerobic

+

+

38.7 ± 1.5

Anaerobic

+

60.2 ± 1.4

Anaerobic

+

+

50.3 ± 2.6

Loblolly pine

Cellic® CTec3

Aerobic

+

84.3 ± 1.2

Anaerobic

+

60.3 ± 0.7