Fig. 6

Mass balance of untreated bagasse and recovered pulp, lignin precipitate and components dissolved in IL after pretreatment at 120 °C for 4 h, shown for whole, industrially depithed and laboratory depithed sugarcane bagasse fractions
Mass balance of untreated bagasse and recovered pulp, lignin precipitate and components dissolved in IL after pretreatment at 120 °C for 4 h, shown for whole, industrially depithed and laboratory depithed sugarcane bagasse fractions