Fig. 2From: Efficient pretreatment of lignocellulosic biomass with high recovery of solid lignin and fermentable sugars using Fenton reaction in a mixed solventEffects of a temperature on the pretreatment of 0.200 g corncob using FeCl3 (7.5 × 10−3 mmol) with H2O2 (35 wt% in H2O, 3.0 mmol, 0.260 mL) in DMSO/water (1:6, 2.0 mL) for 30 min and b reaction time on the pretreatment of 0.200 g corncob using FeCl3 (7.5 × 10−3 mmol) with H2O2 (35 wt% in H2O, 3.0 mmol, 0.260 mL) in DMSO/water (1:6, 2.0 mL) at 130 °CBack to article page