Fig. 3From: Sequential fractionation of the lignocellulosic components in hardwood based on steam explosion and hydrotropic extractionHydrolyzability of the pretreated materials. The conversion efficiencies of SFSTEX (filled circles), SFSTEX+HEX150/8 (filled squares), and SFSTEX+HEX190/4 (empty triangles) are shown. Hydrolysis was conducted with 10 FPU/g cellulose (panel a) and 20 FPU/g cellulose (panel b) as enzyme loadings. The data represent the mean values of four experiments. Error bars indicate the standard deviationBack to article page