Sample | Component recovery in LHW liquid fraction (% of total component amount) | Component recovery in LHW solid fractions (% of total component amount) | Weight loss (DW %) | |||||
---|---|---|---|---|---|---|---|---|
Cellulose | Hemicellulose | Sugar transformation by-products | Cellulose | Hemicellulose | Acid-soluble lignin | Total lignin | ||
TP-120 | 34.9 ± 4.2 | 0 | 16.5 ± 3.8 | 81.8 ± 1.4 | 80.8 ± 2.7 | 71.4 ± 3.6 | 94.6 ± 2.6 | 21.9 ± 1.8 |
TP-160 | 32.9 ± 3.0 | 7.6 ± 1.5 | 17.2 ± 2.0 | 83.9 ± 3.4 | 68.5 ± 3.0 | 69.6 ± 2.7 | 100 ± 5.4 | 24.9 ± 2.4 |
TP-200 | 3.4 ± 0.4 | 11.5 ± 2.4 | 22.5 ± 1.8 | 79.4 ± 3.3 | 42.3 ± 4.5 | 69.2 ± 0.8 | 100 ± 3.9 | 31.5 ± 0.9 |
PT-TP-120 | 2.8 ± 0.7 | 1.9 ± 0.6 | 3.4 ± 0.4 | 75.2 ± 1.0 | 73.5 ± 5.2 | 36.0 ± 3.6 | 87.9 ± 2.0 | 9.1 ± 4.1 |
PT-TP-160 | 2.1 ± 0.1 | 8.9 ± 1.5 | 5.8 ± 0.6 | 62.3 ± 1.6 | 56.9 ± 3.1 | 19.4 ± 1.8 | 75.6 ± 1.7 | 25.8 ± 1.3 |
PT-TP-200 | 0.1 ± 0.04 | 2.4 ± 0.6 | 3.1 ± 0.2 | 67.3 ± 3.1 | 46.1 ± 2.4 | 20.7 ± 1.1 | 80.9 ± 0.7 | 22.9 ± 0.6 |