Skip to main content
Figure 8 | Biotechnology for Biofuels

Figure 8

From: Lignosulfonate-mediated cellulase adsorption: enhanced enzymatic saccharification of lignocellulose through weakening nonproductive binding to lignin

Figure 8

Effect of the pretreatment hydrolysate on glucan conversion of solid substrate SP-Lp-A 1 B 8 and SP-Po-A 1 B 4 . (See Table 3 for details about SP-Lp-A1B8 and SP-Po-A1B4). The enzymatic hydrolysis was conducted at pH 4.8 with Cel dosage of 15 FPU/g glucan and β-glucosidase dosage of 22.5 CBU/g glucan for SP-Lp-A1B8 (0.8 g solid substrate), and 7.5 FPU/g glucan and β-glucosidase 11.25 CBU/g glucan for SP-Po-A1B4 (0.8 g solid substrate). Cel, cellulase; SPORL, sulfite pretreatment to overcome recalcitrance of lignocellulose.

Back to article page