Cellulose (%)
|
Hemicellulose (%)
|
Klason lignin (%)
|
---|
Before pretreatment
|
39.9 ± 0.6
|
20.8 ± 0.3
|
20.7 ± 0.2
|
DA-GJG
|
46.1 ± 0.6
|
15.0 ± 0.7
|
26.9 ± 2.4
|
DA-GJG-DL1
|
58.2 ± 2.5
|
13.4 ± 0.3
|
17.8 ± 0.3
|
DA-GJG-DL2
|
67.7 ± 2.0
|
12.6 ± 0.2
|
9.8 ± 0.7
|
DA-GJG-DL3
|
76.6 ± 0.3
|
11.3 ± 0.2
|
4.1 ± 0.1
|
- DA-GJG-DL represents the DA-GJG treating with sodium chlorite to delignify. The numbers at the end indicate the times of delignification. DA-GJG-DL was only utilized in the experiments as shown in Fig. 6. The compositional analysis was conducted as described elsewhere [43]