Table 1 Particle size distribution, specific surface area, and crystallinity of corn stover samples

From: Structure–property–degradability relationships of varisized lignocellulosic biomass induced by ball milling on enzymatic hydrolysis and alcoholysis

Sample D10 (μm) D50 (μm) D90 (μm) Span SSA (m2 g−1) CrI (%)
BM0 38.17 ± 0.50d 263.00 ± 0.82e 828.33 ± 8.73d 3.00 ± 0.03a 1.12 ± 0.08a 40.68 ± 0.39e
BM10 4.98 ± 0.02c 39.13 ± 0.21d 276.00 ± 2.83c 6.93 ± 0.05f 2.30 ± 0.11b 36.03 ± 0.70d
BM30 1.92 ± 0.01b 11.33 ± 0.95c 42.27 ± 0.95b 3.56 ± 0.07b 3.35 ± 0.11c 20.69 ± 1.27c
BM60 1.20 ± 0.01a 7.18 ± 0.02a 30.10 ± 0.67a 4.03 ± 0.09d 4.07 ± 0.32d 14.06 ± 0.42b
BM90 1.16 ± 0.04a 7.39 ± 0.20a 32.37 ± 0.33a 4.22 ± 0.04e 4.01 ± 0.12d 9.74 ± 0.75a
BM120 1.06 ± 0.01a 7.42 ± 0.04a 32.80 ± 1.61a 4.28 ± 0.19e 4.01 ± 0.03d 9.34 ± 0.72a
BM240 1.32 ± 0.03a 8.90 ± 0.11b 36.40 ± 0.56ab 3.94 ± 0.01 cd 3.75 ± 0.23 cd 7.80 ± 0.45a
BM480 1.38 ± 0.02a 9.08 ± 0.11b 35.67 ± 1.24ab 3.77 ± 0.10c 3.62 ± 0.13 cd 7.45 ± 0.02a
  1. Data are presented as mean ± standard deviation. Values in the same column with different letters are significantly different (p < 0.05)