Raw material

Pre-treatment

Oat hullsa

STEX 185 °C, 7 min, 1% (w/w) H2SO4

Corn stovera

STEX 200 °C, 10 min, 0.2% (w/w) H2SO4

Sugarcane bagassea

STEX 200 °C, 10 min, 0.2% (w/w) H2SO4

Wheat strawa

STEX 190 °C, 10 min, 0.2% (w/w) H2SO4

Spruceb

STEX 205 °C, 7 min, 1.5% (w/w) SO2

Softwood logging residuesb

STEX 205 °C, 7 min, 1.5% (w/w) SO2

Birchb

STEX 200 °C, 5 min, 2.5% (w/w) SO2

  1. a Non-woody hydrolysates. b Woody hydrolysates